As we all know, beauty seam technology can play a very good aesthetic role. If you need to do beauty seam, you must see whether the environment allows the construction.So will the cold weather affect the beauty seam?

In winter, the temperature is low, and the sealant with better quality can be used above 0 degrees, but it is almost less than 10 degrees.So if the temperature is too low, the sealant can be soaked in warm water of 70 to 80 degrees Celsius for ten minutes, so that the sealant will be very easy to play.Northern winter warm, more to do the ceramic tile seam, because do not do the tile grout, the heat produced by the heating will rise from the gap, so as to bring out dust, bacteria.

What are the factors affecting the filling grout

 


 

1, the wind,

The wind in winter is cool, and the air in the north is especially dry. Pay attention to closing the doors and Windows during construction, because the long cool wind is easy to crack the sealant when it is solidified.

Winter in the south of the humidity is heavy, do not open the window before and after the construction of ventilation, clean up the gap, to ensure that no moisture, no water droplets, the gap to keep dry. Avoid the absorption of moisture in the curing agent, appear white, light color.Once there is a whitening phenomenon, it is recommended to shovel off the whitening place and do it again.

2, humidity

The construction environment of sealant should be dry and moisture-proof as far as possible. Many places in south China become cold and wet after winter.There are moisture and water droplets on the wall. Many sealant are easy to turn white after curing in the case of high humidity. If conditions permit, it is best to turn on the air conditioning dehumidification function before construction, and then carry out construction half an hour later.

3. Storage of sealant

Winter sealant storage temperature should be ensured between 5-30, placed in a dry and ventilated place.Avoid low temperatures and humidity.

To sum up, if the temperature is low in winter, good quality sealant can be used above zero, if the quality is not good, it can not be constructed below 10 degrees.Kelin epoxy gap filler manufacturer will give you the best sealant and the best quality service, you are welcome to contact us at any time.